Pitting corrosion behavior and grain evolution of shot peened type 304 stainless steel

T. D. Widodo, K. Noda

Research output: Chapter in Book/Report/Conference proceedingConference contribution

1 Citation (Scopus)

Fingerprint

Dive into the research topics of 'Pitting corrosion behavior and grain evolution of shot peened type 304 stainless steel'. Together they form a unique fingerprint.