Evaluation on tensile creep test of post-installed anchor

Shigehiro Ando, Hiroshi Yamada, Katsuhiko Nakano, Hitoshi Hamasaki, Takehiko Tanuma

研究成果: Article

1 引用 (Scopus)

抄録

The tensile creep test of the post-installed anchor was carried out by the improved spring type creep test equipment. The measurement of creep deformation from non-load and creep fracture time was possible over a long period of time by this equipment. The creep deformation at about 1/3 load of the maximum load increase slightly for the duration of 90 day, but the creep deformation is very small, and creep fracture will not occur in 50 years. And at 80% of the maximum load, creep fracture occurred in 168 days.

元の言語English
ページ(範囲)7-10
ページ数4
ジャーナルAIJ Journal of Technology and Design
21
発行部数47
出版物ステータスPublished - 2015 2 1

Fingerprint

Anchors
Creep

ASJC Scopus subject areas

  • Building and Construction
  • Architecture

これを引用

Ando, S., Yamada, H., Nakano, K., Hamasaki, H., & Tanuma, T. (2015). Evaluation on tensile creep test of post-installed anchor. AIJ Journal of Technology and Design, 21(47), 7-10.

Evaluation on tensile creep test of post-installed anchor. / Ando, Shigehiro; Yamada, Hiroshi; Nakano, Katsuhiko; Hamasaki, Hitoshi; Tanuma, Takehiko.

:: AIJ Journal of Technology and Design, 巻 21, 番号 47, 01.02.2015, p. 7-10.

研究成果: Article

Ando, S, Yamada, H, Nakano, K, Hamasaki, H & Tanuma, T 2015, 'Evaluation on tensile creep test of post-installed anchor', AIJ Journal of Technology and Design, 巻. 21, 番号 47, pp. 7-10.
Ando, Shigehiro ; Yamada, Hiroshi ; Nakano, Katsuhiko ; Hamasaki, Hitoshi ; Tanuma, Takehiko. / Evaluation on tensile creep test of post-installed anchor. :: AIJ Journal of Technology and Design. 2015 ; 巻 21, 番号 47. pp. 7-10.
@article{71ca3f7ef8044448a8f30a728191eb4f,
title = "Evaluation on tensile creep test of post-installed anchor",
abstract = "The tensile creep test of the post-installed anchor was carried out by the improved spring type creep test equipment. The measurement of creep deformation from non-load and creep fracture time was possible over a long period of time by this equipment. The creep deformation at about 1/3 load of the maximum load increase slightly for the duration of 90 day, but the creep deformation is very small, and creep fracture will not occur in 50 years. And at 80{\%} of the maximum load, creep fracture occurred in 168 days.",
keywords = "Bonded anchor, Creep, Creep fracture, Durability, Post-installed anchor",
author = "Shigehiro Ando and Hiroshi Yamada and Katsuhiko Nakano and Hitoshi Hamasaki and Takehiko Tanuma",
year = "2015",
month = "2",
day = "1",
language = "English",
volume = "21",
pages = "7--10",
journal = "AIJ Journal of Technology and Design",
issn = "1341-9463",
publisher = "Architectural Institute of Japan",
number = "47",

}

TY - JOUR

T1 - Evaluation on tensile creep test of post-installed anchor

AU - Ando, Shigehiro

AU - Yamada, Hiroshi

AU - Nakano, Katsuhiko

AU - Hamasaki, Hitoshi

AU - Tanuma, Takehiko

PY - 2015/2/1

Y1 - 2015/2/1

N2 - The tensile creep test of the post-installed anchor was carried out by the improved spring type creep test equipment. The measurement of creep deformation from non-load and creep fracture time was possible over a long period of time by this equipment. The creep deformation at about 1/3 load of the maximum load increase slightly for the duration of 90 day, but the creep deformation is very small, and creep fracture will not occur in 50 years. And at 80% of the maximum load, creep fracture occurred in 168 days.

AB - The tensile creep test of the post-installed anchor was carried out by the improved spring type creep test equipment. The measurement of creep deformation from non-load and creep fracture time was possible over a long period of time by this equipment. The creep deformation at about 1/3 load of the maximum load increase slightly for the duration of 90 day, but the creep deformation is very small, and creep fracture will not occur in 50 years. And at 80% of the maximum load, creep fracture occurred in 168 days.

KW - Bonded anchor

KW - Creep

KW - Creep fracture

KW - Durability

KW - Post-installed anchor

UR - http://www.scopus.com/inward/record.url?scp=84923171796&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84923171796&partnerID=8YFLogxK

M3 - Article

AN - SCOPUS:84923171796

VL - 21

SP - 7

EP - 10

JO - AIJ Journal of Technology and Design

JF - AIJ Journal of Technology and Design

SN - 1341-9463

IS - 47

ER -