Formation of anticorrosive film for suppressing pitting corrosion on Al-Mg-Si alloy by steam coating
Ai Serizawa, Takuhiro Oda, Kohei Watanabe, Kotaro Mori, Tetsuya Yokomizo, Takahiro Ishizaki