A novel process by using chemical leaching followed by bacterial reductive precipitation was proposed for selenium recovery from kiln powder as a byproduct of cement manufacturing. The kiln powder at a slurry concentration of 10 w/v% with 0.25 M Na2CO3 at 28 °C produced wastewater containing about 30 mg-Se/L selenium. The wastewater was diluted four-fold and adjusted to pH 8.0 as preconditioning for bioreduction. A bacterial strain Pseudomonas stutzeri NT-I, capable of reducing selenate and selenite into insoluble elemental selenium, could recover about 90% selenium from the preconditioned wastewater containing selenium of 5 mg-Se/L when supplemented with lactate or glycerol. The selenium concentrations in the treated wastewater were low around the regulated effluent concentration of 0.1 mg-Se/L in Japan.

元の言語English
ページ(範囲)1294-1300
ページ数7
ジャーナルWater Science and Technology
72
発行部数8
DOI
出版物ステータスPublished - 2015 10

ASJC Scopus subject areas

  • Environmental Engineering
  • Water Science and Technology

フィンガープリント Selenium recovery from kiln powder of cement manufacturing by chemical leaching and bioreduction' の研究トピックを掘り下げます。これらはともに一意のフィンガープリントを構成します。

  • これを引用